Guides · Cracks in a new build

Cracks in new build walls: normal shrinkage or a defect?

Fine cracks at wall, floor and ceiling junctions up to 2 mm wide are an expected part of a new home drying out. Wider cracks, cracks that keep growing, diagonal cracks from window and door corners, and cracks in the outside walls are worth measuring, photographing and reporting.

By ARX Algorithms, makers of SnagAudit · Updated 26 October 2026

The short answer

A new home is built with materials that hold a lot of water: plaster, mortar, concrete and timber. As the house is heated and lived in, they dry and shrink, and small cracks appear. NHBC, the UK's largest new home warranty provider, describes small cracks in walls and gaps in joinery as "common signs of shrinkage" and advises leaving them for a few months and filling them once the house has dried out. Its Standards accept cracks up to 2 mm wide at wall, floor and ceiling junctions, and up to 4 mm where a staircase meets a wall.

A crack is worth reporting to the developer when it is wider than those figures, is getting wider, runs diagonally from the corner of a window or door, appears on the outside of the house, or comes with doors and windows that start to stick. Report it in writing within the two-year builder warranty period, with a measurement and dated photographs.

What the standards say is acceptable

NHBC Standards chapter 9.1, "A consistent approach to finishes", is the benchmark most developers and warranty providers work to:

WhereWhat NHBC accepts
Wall, floor and ceiling junctions insideSome cracking up to 2 mm wide, from movement and shrinkage of materials
Where a staircase string meets a wallA crack up to 4 mm from shrinkage
Unplastered garage blockworkCracks up to 2 mm from thermal movement and shrinkage
Brick and block mortar jointsSome minor shrinkage cracking between units and joints
Facing brickwork outsideNo significant cracks in the facing bricks, judged from at least 10 m in daylight
RenderFree from crazing (hairline cracks wider than 0.2 mm); some localised hairline cracking is acceptable if it does not affect performance

Developers publish similar thresholds. Redrow, for example, asks homeowners to tell it about cracks wider than 2 mm (4 mm on the staircase), and says it will deal with cracks round skirting boards wider than that under the warranty. Smaller cracks are treated as part of normal maintenance.

How serious is a crack? The BRE categories

Surveyors and engineers in the UK grade visible cracking using BRE Digest 251, Assessment of damage in low-rise buildings. The categories are based mainly on how easy the damage is to repair, with crack width as a guide:

CategoryTypical crack widthWhat it means
0: HairlineUp to 0.1 mmAesthetic. Redecoration only.
1: FineUp to 1 mmAesthetic.
2: Easily filledUp to 5 mmAesthetic. BRE says categories 0 to 2 "require only redecoration".
3: Some opening up needed5 to 15 mmServiceability: can affect weather-tightness and doors and windows.
4: Extensive damage15 to 25 mmServiceability.
5: StructuralOver 25 mmStability: likely to need structural work.

BRE stresses that width is not the whole story: whether a crack is still growing matters too, and a building professional should be consulted where damage is significant. In a new build, anything in category 3 or above, or any crack that keeps widening, should go to the developer and, if the builder warranty period has ended, to the warranty provider.

Shrinkage crack or something more?

Usually shrinkage

Worth reporting now

How to measure and record a crack

  1. Measure the width at the widest point. A crack-width gauge costs a few pounds; otherwise a steel rule, or coins of known thickness, give a reasonable guide. Note the length and direction (horizontal, vertical, diagonal, stepped).
  2. Photograph it twice: close up with the rule or gauge in shot, and from further back so the location is obvious.
  3. Mark the ends lightly in pencil with the date. If the crack grows past the marks, that is evidence it is moving.
  4. Re-check every few weeks, from the same spot, and keep each set of photographs together.
  5. Report it in writing with the measurements and photographs. Our guide to getting new build defects fixed covers the steps and deadlines.

Who fixes cracks, and when

In the first two years after completion, the developer is responsible for defects that breach the warranty's technical standards. Cracks within the NHBC tolerances are normally treated as the homeowner's maintenance: NHBC's own advice is to fill them with a good filler when you redecorate, and to wait about 9 to 12 months before applying further coats of paint or wallpaper. Whether your developer will fill shrinkage cracks at all is set by its own after-sales policy, so check its homeowner guide rather than assuming.

From year 3, warranty insurance covers damage from defects in specified parts of the home, usually the structure. LABC Warranty, for example, excludes cosmetic issues and snagging. Fine shrinkage cracks will not be covered at that stage, but structural cracking can be. Use our deadlines calculator to see exactly when your two-year period ends.

Keeping drying-out cracks to a minimum

Recording cracks with SnagAudit

In the SnagAudit snagging app each crack is a numbered item with its room, exact location and a "measured against tolerance" note such as "2.5 mm at wall and ceiling junction (tolerance 2 mm, NHBC 9.1)". Draw an arrow or circle on the photograph, and every photo is timestamped and hashed at capture. A re-inspection a few weeks later carries the item forward with the original photographs, so the report shows whether the crack has grown.

Sources

Questions

Are cracks normal in a new build?

Yes. Fine cracks at wall, floor and ceiling junctions and gaps in joinery are common as a new home dries out. NHBC Standards accept cracks up to 2 mm wide at junctions and up to 4 mm where the staircase meets a wall.

What size crack in a new build should I worry about?

Report anything wider than 2 mm inside (4 mm by the stairs), any crack that keeps widening, diagonal cracks from window and door corners, cracks in the outside walls, and anything accompanied by sticking doors or windows. Cracks over 5 mm fall into BRE category 3 or higher.

Will the builder fix shrinkage cracks?

Cracks within the NHBC tolerances are generally treated as normal maintenance; whether a developer will fill them is set by its own after-sales policy. Cracks beyond tolerance should be reported in writing within the two-year builder warranty period.

How long does a new build take to dry out?

NHBC does not give a single figure, but advises leaving cracks for a few months before filling them and waiting about 9 to 12 months before further coats of paint or wallpaper.

Does the 10-year warranty cover cracks?

From years 3 to 10 the warranty covers damage from defects in specified parts of the home, usually the structure. Cosmetic cracking and snagging are typically excluded, and a minimum claim value or excess applies.